Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00150 - 0.00170 GPa | 0.218 - 0.247 ksi | DIN 53504 S2 |
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |