Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0190 GPa | 2.76 ksi | ASTM D412 |
Precision Polymer Engineering Perlast® G90A Perfluoroelastomer A black general purpose perfluoroelastomer compound with exceptionally high chemical resistance and excellent steam resistance and mechanical properties. Extremely low outgassing properties.Applicat.. |
|||
100% Modulus | 0.0190 GPa | 2.76 ksi | ISO 37 |
Huntsman AVALON® 60 DB Thermoplastic Polyurethane Introduction: AVALON 60 DB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DB is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
100% Modulus | 0.0190 GPa | 2.76 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® D16N60D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 16N60D is a polyether-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining high hardness with excellent mechanical properties and .. |
|||
100% Modulus | 0.0190 GPa | 2.76 ksi | ASTM D412 |
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 70DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig.. |
|||
100% Modulus | 0.0190 GPa | 2.75 ksi | ASTM D-638 |
Axiall 21540 Coax & Telecom Flexible PVC Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation.Information provided by Georgia GulfGeorgi.. |
|||
100% Modulus | 0.0190 GPa | 2.75 ksi | ASTM D-638 |
Axiall 21540 Coax & Telecom Flexible PVC Black 307 Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation. Max service temperature rating of 80°C .. |
|||
100% Modulus | 0.0190 GPa | 2.75 ksi | ASTM D-638 |
Axiall 21570 Coax & Telecom Flexible PVC Semi-rigid insulation compound designed for data communication riser cable applications. Maximum 75°C service temperature rating.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp.. |
|||
100% Modulus | 0.0190 GPa | 2.76 ksi | ASTM D412 |
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |