Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0170 GPa | 2.47 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® Activa D126K BL Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLCOAT® Activa D126K BL is a standard polyester based TPU, supplied in form of translucent, black colored pellets, combining hardness with excellent low-temperature flexibility. PEARLCOAT® Acti.. |
|||
100% Modulus | 0.0170 GPa | 2.47 ksi | ISO 37 |
Huntsman AVALON® 60 DE Thermoplastic Polyurethane Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
100% Modulus | 0.0170 GPa | 2.47 ksi | ISO 37 |
Huntsman AVALON® 98 AB Thermoplastic Polyurethane Introduction: AVALON 98 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 98 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
100% Modulus | 0.0170 GPa | 2.47 ksi | DIN 53504 |
Huntsman IROGRAN® A 98 E 4735 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
100% Modulus | 0.0170 GPa | 2.47 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1198 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0170 GPa | 2.47 ksi | ISO 37 |
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
100% Modulus | 0.0170 GPa | 2.47 ksi | ISO 37 |
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |