Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0169 GPa | 2.45 ksi | ASTM D412 |
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry application.. |