Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-550D Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.0152 GPa | 2.21 ksi | |
Spartech E65595 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D412 |
Lubrizol Estane® ALR E60D Thermoplastic Polyurethane Type: Estane® ALR E60D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D412 |
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Profile, Cable Jacket; Injection.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | |
Colorite Polymers Self Frosting™ 9011SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D638 |
Colorite Polymers 9000 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | |
Colorite Polymers 9011 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | |
Colorite Polymers 9012 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D638 |
Colorite Polymers 9033 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D638 |
Colorite Polymers 9034 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D638 |
Colorite Polymers 9226 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D-638 |
Axiall 35551 Wire & Cable Flexible PVC TW, THW insulation compound suitable for 105°C AWM applications. Oil II rated and VW-1. CSA approved for TR64, TR32, TEW, and AW.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D-638 |
Axiall 8950 Moldings & Extrusions Flexible PVC General purpose semi-rigid extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D412 |
ACC SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer EP 1009, “Powered by Reactamine®Technology”, is a two component 100% solid Silicone Modified Polyurea with superior performance in industrial applications. EP 1009 displays extremely fast cure ti.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D638 |
Bayshore Vinyl Compounds BVC 4200-90 Vinyl Compound Information Provided by Bayshore Vinyl Compounds Inc. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D-638 |
Axiall 19890 Wire & Cable Flexible PVC Highly recommended for 105°C, 15 mil wall insulations and jackets where good gasoline and oil resistance is desired.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D412 |
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D-638 |
Axiall 22912 Coax & Telecom Flexible PVC Non-lead stabilized, 75C rated jacket compound suitable for CM, CL2 constructions over HDPE primaries. Also suitable for riser applications over FR PVC primaries.Information provided by Georgia Gul.. |
|||
100% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D-638 |
Axiall 8911 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound. UV stabilized.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |