Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | >= 0.0100 GPa | >= 1.45 ksi | DIN 53504 |
NEXA® PFX8010 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | DIN 53504 |
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 95 R 4813 is a thermoplastic polyester- polyurethane for injection moulding applications. Additional characteristics of the product are very short cycle times and high dimens.. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11T92E Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11T92E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 15N95UV is a polyether copolymer-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resist.. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D412 |
Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding TPU properties.Uses: Cable jacket and tube/hos.. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-7190 Polycaprolactone Based TPU Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8190 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8254 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | DIN 53504 |
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ISO 37 |
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D412/D638 |
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane Features: Hard, flexible, abrasion resistant coatings. Primarily used for all solution binder for inks and lacquers on fabrics and various substrates.Uses: Adhesives and inks & lacquers, pigment bin.. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | JIS-A-5756 |
Denka VINYKON M557050 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D-638 |
Axiall 10790 Wire & Cable Flexible PVC 60C compound suitable for integral non-metallic conduit jacket 1" and larger per UL 1660.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D-638 |
Axiall 69148 Wire & Cable Flexible PVC Non-lead stabilized tray cable jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D-638 |
Axiall 830B Wire & Cable Flexible PVC 80°C rated compound recommended for UL 360, liquid tight flexible conduit jacket applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D-638 |
Axiall 8835 Moldings & Extrusions Flexible PVC General purpose extrusion compound with low gloss surface finish.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D-638 |
Axiall 19853 Wire & Cable Flexible PVC Non-lead stabilized insulation compound recommended for 105°C applications 1/32 wall and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2195 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.0100 GPa | 1.45 ksi | ASTM D-638 |
Axiall 38511 Wire & Cable Flexible PVC Tray cable jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |