Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D412 |
S&E Specialty Polymers G-3085E PVC Application: General purpose PVC material with good low temperature properties designed for T-Molding extrusion applicationsInformation provided by S&E Specialty Polymers |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | |
Dow Pellethane® 2103-90AEF Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2103-90AEF elastomer is a polytetramethylene glycol ether based polyurethane elastomer, featuring superior resilience, low temperature properties, excellent hydrolytic stability, and re.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | |
Dow Pellethane® 2103-90AEN Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2103-90AEN is a polytetramethylene glycol ether based polyurethane elastomer featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 16N92 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 16N92 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resistance. It can b.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | 25 mil film; ASTM D412 |
Huntsman IROGRAN® A 95 P 5003 TPU-Polyether IROGRAN® A 95 P 5003 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications.Information provided by Alliance Polymers |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | |
Spartech M60480 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D412 |
SK Chemicals SKYTHANE® R190A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D638 |
Colorite Polymers 7502 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D638 |
Colorite Polymers 8200FR General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D-638 |
Axiall EX 3114B Plenum Flexible PVC Non-lead stabilized CAT 3 jacket recommended for hybrid constructions. Also recommended for 25+ pair counts.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D-638 |
Axiall EX1188A Wire & Cable Flexible PVC UL 360 jacket compound. 80°C air; 60°C oil.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D412 |
ACC EP RSP-AL EPI Engineered Polymers Aromatic Silicone Polyurea EP RSP-AL, Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea. This increases UV resistance without sacrificing physical properties. EP RSP-AL.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D-638 |
Axiall 38552 Wire & Cable Flexible PVC General purpose insulating and jacketing compound for 105°C AWM and SPT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D-638 |
Axiall 38601 Coax & Telecom Flexible PVC CATV and general purpose jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D-638 |
Axiall 830 Wire & Cable Flexible PVC TW insulation. UL recognized for TW and Oil resistant II.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D-638 |
Axiall 8803 Moldings & Extrusions Flexible PVC Microbe resistant extrusion and molding compound designed for use in weatherstrips, screen spline and flexible gaskets. Good UV resistance.Information provided by Georgia GulfGeorgia Gulf became Ax.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D-638 |
Axiall 8900 Moldings & Extrusions Flexible PVC General purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D412 |
ACC EP RSP EPI Engineered Polymers Silicone Polyurea EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure time.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D-638 |
Axiall 2192 Wire & Cable Flexible PVC Non-lead stabilized SJTO, SJTOO oil resistant flexible cord jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D638 |
Colorite Polymers 8007SF General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ASTM D-638 |
Axiall 8843 Moldings & Extrusions Flexible PVC General purpose, non-lead stabilized extrusion compound. Well suited for 80°C rated automotive tubing.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | ISO 37 |
PolyOne Elastamax XL 0254-15 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a urethane based thermoplastic elastomer specially lubricated for auto suspension bushings. Physical Form: Pellets. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hann.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00896 GPa | 1.30 ksi | |
Dow Pellethane® 2354-45D Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2354-45D elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyurethane.. |