Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7010-40D Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D638 |
Colorite Polymers 8088 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D-638 |
Axiall 18770 Moldings & Extrusions Flexible PVC General purpose 105C, clear jacketing compound recommended for 1/32" wall and larger. Exhibits excellent migration properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D-638 |
Axiall 8801 Moldings & Extrusions Flexible PVC General purpose clear extrusion compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D-638 |
Axiall 19840 Wire & Cable Flexible PVC 105°C rated insulation suitable for 1/64 wall. Recommended for AWM applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D638 |
Colorite Polymers 8000 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D638 |
Colorite Polymers 8002 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |