Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00810 GPa | 1.17 ksi | Press cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 232°C |
3M Dyneon™ 2299X Ultra High Viscosity Fluoroelastomer 3M™ Dyneon™ FC 2299X is an ultra high viscosity fluoroelastomers designed for use in applications such as o-rings, gaskets and seals requiring higher strength than achievable with lower viscosity .. |
|||
100% Modulus | 0.00810 GPa | 1.17 ksi | Press cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 232°C |
3M Dyneon™ 2299PX Ultra High Viscosity Fluoroelastomer 3M™ Dyneon™ FC 2299PX is an ultra high viscosity fluoroelastomers designed for use in applications such as o-rings, gaskets and seals requiring higher strength than achievable with lower viscosity.. |