Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00770 GPa | 1.12 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4190 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4190 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
100% Modulus | 0.00770 GPa | 1.12 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4490 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4490 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |
|||
100% Modulus | 0.00770 GPa | 1.12 ksi | Heat aged 2 weeks at 175°C |
DuPont Vamac® DP Activator OC Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
100% Modulus | 0.00770 GPa | 1.12 ksi | ISO 37 |
AlphaGary Evoprene™ 029 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |