Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00680 GPa | 0.986 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00680 GPa | 0.986 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-390A Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.00680 GPa | 0.986 ksi | Press-cured 5 minutes at 190°C |
DuPont Vamac® DP HVA-2 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
100% Modulus | 0.00680 GPa | 0.986 ksi | Air aged 7 days at 150°C |
DuPont Vamac® GLS Sample Compound Vulcanizate Slab Cured Test slab is press cured for 5 minutes at 177°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for thei.. |
|||
100% Modulus | 0.00680 GPa | 0.986 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00680 GPa | 0.986 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR8520 Standard Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00680 GPa | 0.986 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR9060EF PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |