Polymer Property : 100% Modulus = 0.00630 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00630 GPa
0.914 ksi
12.5% change after 72 hours @ 200°C; ASTM D412
Precision Polymer Engineering Perlast® G80X Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require exposure..
100% Modulus 0.00630 GPa
0.914 ksi
Freudenberg Simrit Superiorâ„¢ F850 Fluoroelastomer
Cost-effective, high performance compound for semiconductor applications. Superior F850 offers outstanding plasma resistance and low particulation in a wide range of plasma environments.
100% Modulus 0.00630 GPa
0.914 ksi
DIN 53504
Lubrizol ESTANE® T5213 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00630 GPa
0.914 ksi
DIN 53504
Lubrizol ESTANE® 58564 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00630 GPa
0.914 ksi
ISO 37
AlphaGary Evoprene™ 032 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
100% Modulus 0.00630 GPa
0.914 ksi
Post cure 2 hours @ 232°C
3M Dyneon™ FPO 3740 Fluoroelastomer
3M™ Dyneon™ FPO 3740 is a peroxide curable fluoroelastomer terpolymer containing 69.5 wt% fluorine. FPO 3740 can be used in compression, transfer or injection molding, and extrusion processes. Fea..
100% Modulus 0.00630 GPa
0.914 ksi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8605 (GF-S) Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued **