Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00538 GPa | 0.781 ksi | |
Taiwan Sheen Soon Sheenthane® A8556K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00538 GPa | 0.781 ksi | DCBP Cure |
Shin-Etsu Silicones SV-18000U Silicone Rubber SV18000U is one of a series of easy processing, mineral filled silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Fe.. |
|||
100% Modulus | 0.00538 GPa | 0.780 ksi | ASTM D412 |
SK Chemicals SKYTHANE® L185A Polycaprolactone Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.00538 GPa | 0.780 ksi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 1070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00538 GPa | 0.780 ksi | Press Cure 15 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FLS 2650 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FLS 2650 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |