Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00527 GPa | 0.765 ksi | ASTM D412 |
SK Chemicals SKYTHANE® R180A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.00527 GPa | 0.765 ksi | ASTM D638 |
Bayshore Vinyl Compounds BVC 7200-75 Vinyl Compound BVC 7200-75 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a s.. |
|||
100% Modulus | 0.00527 GPa | 0.764 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00527 GPa | 0.764 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |