Mechanical Properties Metric English Comments
100% Modulus 0.00362 GPa
0.525 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.25 PHR Zinc Stearate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00362 GPa
0.525 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00362 GPa
0.525 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00362 GPa
0.525 ksi
ASTM D-638
Axiall 8610 Moldings & Extrusions Flexible PVC
A high quality, low gravity, clear extrusion and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00362 GPa
0.525 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.25 PHR Zinc Stearate
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00362 GPa
0.525 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00362 GPa
0.525 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00362 GPa
0.525 ksi
ASTM D-638
Axiall 18660 Moldings & Extrusions Flexible PVC
Flame retardant extrusion and molding compound recommended for 105C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.