Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00343 GPa | 0.498 ksi | |
Taiwan Sheen Soon Sheenthane® A7020 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
100% Modulus | 0.00343 GPa | 0.497 ksi | |
Taiwan Sheen Soon Sheenthane® A7530 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00343 GPa | 0.497 ksi | |
Taiwan Sheen Soon Sheenthane® A7630 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00343 GPa | 0.498 ksi | |
Taiwan Sheen Soon Sheenthane® A7710 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
100% Modulus | 0.00343 GPa | 0.498 ksi | |
Taiwan Sheen Soon Sheenthane® A7711 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
100% Modulus | 0.00343 GPa | 0.498 ksi | |
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
100% Modulus | 0.00343 GPa | 0.498 ksi | |
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
100% Modulus | 0.00343 GPa | 0.498 ksi | |
Taiwan Sheen Soon Sheenthane® A7810L TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
100% Modulus | 0.00343 GPa | 0.497 ksi | |
Taiwan Sheen Soon Sheenthane® A8760 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00343 GPa | 0.497 ksi | |
Taiwan Sheen Soon Sheenthane® A8760F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00343 GPa | 0.498 ksi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 155 FT SWB Thermoplastic Vulcanizate Neoplast 155 FT SWB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant,.. |
|||
100% Modulus | 0.00343 GPa | 0.498 ksi | Parallel Flow; ASTM D412 |
Advanced Polymer Alloys DuraGrip™ 6165 TR Thermoplastic Elastomer DuraGrip® DGR6165TR is a translucent thermoplastic elastomer (TPE) formulated for excellent elastic properties and enhanced adhesion to engineered thermoplastics using insert molding, co-injection .. |