Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00280 GPa | 0.406 ksi | ISO/R527 |
Polykemi AB POLYelast TPE E706 Thermoplastic Elastomer, EPDM-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | ASTM D638 |
Multibase Multi-Flex® TPE A 5801 LC BLK Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and fe.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | ASTM D412 |
UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8068B Thermoplastic Elastomer Elastocon® 8068B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068B is well suited for consumer goods an.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | |
Dow AFFINITY™ EG 8150 Polyolefin Elastomer AFFINITY® EG 8150 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation It ex.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | |
Dow AFFINITY™ EG 8200 Polyolefin Elastomer AFFINITY® EG 8200 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation. It e.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | ASTM D412 |
Advanced Polymer Alloys Alcryn® 2170 NC Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | ASTM D412 |
Advanced Polymer Alloys DuraGrip™ DGR 6170 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6170 is offered in an NC (colorable) version, and is designed to chemically bond to a wide variety of thermoplastic substrates including ABS, PC, Nylon 6,
Nylon 6/6, glass filled Nylo.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | ASTM D412 |
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane Features: Excellent blend partner for PVC and general adhesive and good physical properties.Uses: Flat die/cast film extrusion and hose jacketing, Calendaring/melt coating.Available in Americas, Eur.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | ASTM D412; ASTM D638 |
Lubrizol Estane® 58252 Thermoplastic Polyurethane Type: Estane® 58252 is a 70A polyether-type thermoplastic polyurethane (TPU).Features: Formulated to have one of the highest MVT values within the thermoplastic polyurethane class. It is also amon.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Gum Compound
(discontinued **)& Gum compound with 100 parts Hypalon; 4 parts high activity magnesia; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont Dow Elastomers). Physical property data below (.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5683 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
100% Modulus | 0.00280 GPa | 0.406 ksi | ISO 37 |
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |