Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00270 GPa | 0.392 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00270 GPa | 0.392 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 4.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00270 GPa | 0.392 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
100% Modulus | 0.00270 GPa | 0.392 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4465 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4465 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
100% Modulus | 0.00270 GPa | 0.392 ksi | |
DuPont Vamac® GXF Sample Compound Vulcanizate Slab Cure (5 minutes at 190°C) Test slab is cured for 5 minutes at 190°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for their own .. |
|||
100% Modulus | 0.00270 GPa | 0.392 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00270 GPa | 0.392 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 4.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00270 GPa | 0.392 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00270 GPa | 0.392 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® STK55PA Thermoplastic Elastomer Elastocon® STK55PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK55PA is well suited for consumer go.. |
|||
100% Modulus | 0.00270 GPa | 0.392 ksi | ISO 37 |
AlphaGary Evoprene™ COGEE 683 SEBS Thermoplastic Elastomer Evoprene™ COGEE was developed to comold or coextrude with engineered thermoplastics and designed for soft touch applications.Processing: compatible with polypropylene and polystyrene for co-molding.. |
|||
100% Modulus | 0.00270 GPa | 0.392 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00270 GPa | 0.392 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5650 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |