Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00269 GPa | 0.390 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 350ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00269 GPa | 0.390 ksi | ASTM D412 |
Teknor Apex TELCAR® 1050-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00269 GPa | 0.390 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, 350ºF Cure Temperature MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00269 GPa | 0.390 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 82A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00269 GPa | 0.390 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00269 GPa | 0.390 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 82A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
100% Modulus | 0.00269 GPa | 0.390 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |