Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00259 GPa | 0.375 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 350ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00259 GPa | 0.375 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 350ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00259 GPa | 0.376 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Translink 555 Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00259 GPa | 0.375 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00259 GPa | 0.375 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Mistron Vapor Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00259 GPa | 0.375 ksi | Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FE 5730 Fluoroelastomer Composition: Ter-polymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethyleneLower fluorine version of FE 5830QProcess targets: extrusion onlyProprietary incorporated cure technologyP.. |
|||
100% Modulus | 0.00259 GPa | 0.375 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00259 GPa | 0.376 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Translink 555 Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00259 GPa | 0.375 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Mistron Vapor Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |