Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00245 GPa | 0.355 ksi | ISO 37 |
PolyOne Elastamax XL 1092-2 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on modified TPU technology. Physical Form: Pellet. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hanna and Geon merged.. |
|||
100% Modulus | 0.00245 GPa | 0.355 ksi | |
Taiwan Sheen Soon Sheenthane® A7090 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00245 GPa | 0.356 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Thanecure ZM Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
100% Modulus | 0.00245 GPa | 0.356 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Thanecure ZM Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |