Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00240 GPa | 0.348 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z600A Thermoplastic Elastomer, SEBS-based, Co-injection Grade Information provided by Polykemi AB |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | ISO 37 |
Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4155 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4155 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | Conductive CR Conveyor Belt Cover Compound |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | DIN 53504 |
Lubrizol ESTANE® 5702F3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | ASTM D412 |
UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | DIN 53504 |
Lubrizol ESTANE® 5702F2 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | 500 mm/min, measured parallel to flow; ISO 37 |
AlphaGary Evoprene™ LF 6152 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | ASTM D412 |
Advanced Polymer Alloys Alcryn® 2160 NC Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | ASTM D412 |
Advanced Polymer Alloys DuraGrip™ 6870 Thermoplastic Elastomer With its true rubber look and feel, DuraGrip® TPE improves the performance and appearance of virtually any consumer or light industrial product. Its one of the most versatile materials in APAs exte.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5690 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
100% Modulus | 0.00240 GPa | 0.348 ksi | 500 mm/min, measured parallel to flow; ISO 37 |
AlphaGary Evoprene™ GF 6255 Automotive Thermoplastic Elastomer Evoprene™ GF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |