Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-1052-55 PVC Compound Application: A 105°C scuff, oil and flame resistant high flow molding compound designed for grommets.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 63A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7010-55 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 63A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Lubrizol Estane® ALR E72A Thermoplastic Polyurethane Type: Estane® ALR E72A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Lubrizol Estane® ALR PC73A Thermoplastic Polyurethane Type: Estane® ALR PC73A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | cured 7 mins @ 150°C |
ACC QSil 550R QSI Quantum Silicones Silicone Potting Material QSil 550Ris a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairab.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | cured 20 mins @ 150°C |
ACC QSil 550SB QSI Quantum Silicones Self-Priming Silicone Potting Material QSil 550SB is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repair.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D638 |
Colorite Polymers 5002 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00207 GPa | 0.300 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |