Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00193 GPa | 0.280 ksi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 429 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
100% Modulus | 0.00193 GPa | 0.280 ksi | Injection molded plaques, Die C, Machine Direction; ASTM D412 |
Kraton® G2705 GU (SEBS) Compound Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good punct.. |
|||
100% Modulus | 0.00193 GPa | 0.280 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2250 UT Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |