Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00165 GPa | 0.239 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Oyster Shell Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00165 GPa | 0.240 ksi | ASTM D412-98 |
Saint-Gobain Tygon® 2001 Plasticizer Free Tubing Formulation Description: Tygon® 2001: Tygon® Plasticizer Free Tubing is a uniquely engineered product that offers the low compression set properties of a thermoset rubber. Tygon® Plasticizer Free Tub.. |
|||
100% Modulus | 0.00165 GPa | 0.239 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Oyster Shell Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00165 GPa | 0.240 ksi | ASTM D 412 |
CPT C-Flex® R70-072 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
100% Modulus | 0.00165 GPa | 0.240 ksi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 2250 UT Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |