Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | Original Properties; ASTM D412 Die C |
Freudenberg Simrit S50 Silicone Elastomer (VMQ) General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Non-Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Non-Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00155 GPa | 0.225 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |