Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.000827 GPa | 0.120 ksi | ASTM D412 |
Teknor Apex Uniprene® 35A Polyvinyl Chloride, Flexible Features: High Elastic RecoveryInformation Provided by Teknor Apex |
|||
100% Modulus | 0.000827 GPa | 0.120 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 2023 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.000827 GPa | 0.120 ksi | ASTM D 412 |
CPT C-Flex® R70-028 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
100% Modulus | 0.000827 GPa | 0.120 ksi | ASTM D 412 |
CPT C-Flex® R70-081 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |