Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.000810 GPa | 0.117 ksi | ASTM D412 |
BASF Master Builders Solutions ChemRex® CX-26 Isocyanate-Free Polyurethane-Based Sealant
(discontinued **)< CX-26 is a polyurethane based one-component, moisture curing sealant. It provides fast cure, non-sag, excellent adhesion and has elastomeric properties with high strength which can reduce/eliminate.. |