Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 11.3 J @Temperature 23.0 °C |
8.33 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used.. |