Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 42.0 J @Temperature 23.0 °C |
31.0 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron Magnum™ 358HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Impact Test | 42.0 J @Temperature 23.0 °C |
31.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Diamond Polymers Centrex® 925 Injection Molding Grade Centrex 925 resin is a soft-flow, high-gloss, molding grade of Polycarbonate / ASA (acrylonitrile-styrene-acrylate) blend. It is an injection molding grade with a good balance of physical properties.. |
|||
Impact Test | 42.0 J @Temperature 23.0 °C |
31.0 ft-lb @Temperature 73.4 °F |
High speed instrumented impact (puncture); Energy @ max load; ASTM D3763 |
Diamond Polymers NPP 60-1010 PCTA Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Impact Test | 42.0 J @Diameter 25.4 mm, Temperature 100 °C |
31.0 ft-lb @Diameter 1.00 in, Temperature 212 °F |
bar. 310 HB. |
Assab Steels 618 Plastic Mold Material ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu.. |