Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 5.00 J @Temperature -30.0 °C |
3.69 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
Diamond Polymers Centrex® 925 Injection Molding Grade Centrex 925 resin is a soft-flow, high-gloss, molding grade of Polycarbonate / ASA (acrylonitrile-styrene-acrylate) blend. It is an injection molding grade with a good balance of physical properties.. |
|||
Impact Test | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Dow Retain® 8209 ABS + Polycarbonate Data provided by Dow Chemical. |
|||
Impact Test | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
Multi-axial, at max. load; ASTM D3763 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 5.00 J @Temperature 23.0 °C |
3.69 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Verton RV004ESV_GY7E070 PA 66 Preliminary data for 20% long glass fiber filled, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |