Mechanical Properties Metric English Comments
Impact Test 4.50 J

@Temperature 23.0 °C
3.32 ft-lb

@Temperature 73.4 °F
Multi-axial, at failure, measured on flat plaques; ASTM D3763
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 4.50 J

@Temperature 23.0 °C
3.32 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness)
AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 4.50 J

@Temperature 23.0 °C
3.32 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..