Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 40.0 J @Temperature -30.0 °C |
29.5 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® C1950 PC+ABS Low viscosity injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 40.0 J @Temperature -30.0 °C |
29.5 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 40.0 J @Temperature -30.0 °C |
29.5 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS (Asia Pacific) Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Impact Test | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact; Total Energy; ASTM-D3763 |
Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
Impact Test | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
Multiaxial Impact; E-fail; 0.100 in. thickness, 1.57 in. ring, 0.5 in. dart, 3.46 m/s velocity |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Impact Test | 40.0 J @Temperature -20.0 °C |
29.5 ft-lb @Temperature -4.00 °F |
Total Penetration Energy; ISO 6603-2 |
Borealis Bormod™ BE961MO Polypropylene for Injection Molding Bormod BE961MO is an heterophasic copolymer characterized by an optimum combination of high stiffness, low creep and very high impact strength.Bormod BE961MO is a new generation grade for very fast .. |
|||
Impact Test | 40.0 J @Temperature 0.000 °C |
29.5 ft-lb @Temperature 32.0 °F |
ASTM D3763 |
Diamond Polymers Centrex® 810 Injection Molding Grade Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and .. |
|||
Impact Test | 40.0 J @Thickness 4.00 mm |
29.5 ft-lb @Thickness 0.157 in |
Multi-axial, total energy; ISO 6603-2 |
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Impact Test | 40.0 J @Temperature 23.0 °C |
29.5 ft-lb @Temperature 73.4 °F |
|
Assab Steels ASP 23 Cold Work Steel ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:High wear resistance (abrasive profile)High compressive strengthVery good through-hardening prope.. |