Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 25.0 J @Temperature -20.0 °C |
18.4 ft-lb @Temperature -4.00 °F |
Instrumental Falling Weight - Total Penetration Energy; ISO 6603-2 |
Borealis Bormed™ BE860MO Polypropylene Copolymer for Healthcare Applications Bormed BE860MO is a heterophasic copolymer characterized by an excellent impact strength also at low temperatures (deep freeze applications) together with high stiffness and good flow properties.Bor.. |
|||
Impact Test | 25.0 J @Temperature -20.0 °C |
18.4 ft-lb @Temperature -4.00 °F |
Instrumental Falling Weight - Total Penetration Energy; ISO 6603-2 |
Borealis Bormed™ HD850MO Polypropylene Copolymer for Healthcare Applications Bormed HD850MO is a medium melt flow rate polypropylene homo polymer using the Borealis Nucleation Technology (BNT). This provides a polypropylene with excellent dimensional stability and its high c.. |
|||
Impact Test | 25.0 J @Diameter 25.4 mm, Temperature 20.0 °C |
18.4 ft-lb @Diameter 1.00 in, Temperature 68.0 °F |
310 HB |
Assab Steels 618 Plastic Mold Material ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu.. |