Mechanical Properties Metric English Comments
Impact Test 2.60 J

@Temperature 23.0 °C
1.92 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 2.60 J

@Temperature 23.0 °C
1.92 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 2.60 J

@Temperature 23.0 °C
1.92 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Impact Test 2.60 J

@Temperature 23.0 °C
1.92 ft-lb

@Temperature 73.4 °F
Multi-axial, at max. load; ASTM D3763
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..