Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 1.10 J @Temperature -40.0 °C |
0.811 ft-lb @Temperature -40.0 °F |
ASTM D3763 |
Diamond Polymers Centrex® HGM Automotive Grade, Injection Molding Grade Centrex HGM resin is an exceptionally high-gloss grade of ASA (acrylonitrile-styrene-acrylate). This injection molding grade has excellent gloss retention, excellent resistance to chemicals and high.. |