Mechanical Properties Metric English Comments
Impact Test 81.3 J

@Thickness 3.17 mm,
Temperature -40.0 °C
60.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil LL 8555.24 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 81.3 J

@Thickness 3.17 mm,
Temperature -40.0 °C
60.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil LL 8555.25 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 81.3 J

@Thickness 3.17 mm,
Temperature -40.0 °C
60.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 81.3 J

@Thickness 3.17 mm,
Temperature -40.0 °C
60.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 81.3 J

@Thickness 3.17 mm,
Temperature -40.0 °C
60.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 81.3 J

@Thickness 3.17 mm,
Temperature -40.0 °C
60.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 81.3 J

@Thickness 3.17 mm,
Temperature -40.0 °C
60.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil LLP8555.24 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 81.3 J

@Thickness 3.17 mm,
Temperature -40.0 °C
60.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil LLP8555.25 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Impact Test 81.3 J

@Thickness 3.17 mm,
Temperature -40.0 °C
60.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil LL 8555.67 Rotational Molding Resin  (discontinued **)
LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir..
Copyright © lookpolymers.com All Rights Reserved