Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 46.4 J @Thickness 3.17 mm, Temperature -40.0 °C |
34.2 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D3763 |
ExxonMobil PP8244E1 Polypropylene Homopolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection molded applications requiring excellent processing attributes.Availability: North America Features:Bala.. |