Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 4.70 J @Temperature 23.0 °C |
3.47 ft-lb @Temperature 73.4 °F |
Multi-axial, at failure, measured on flat plaques; ASTM D3763 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 4.70 J @Temperature 23.0 °C |
3.47 ft-lb @Temperature 73.4 °F |
Multi-axial, at failure, measured on flat plaques; ASTM D3763 |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 4.70 J @Temperature 23.0 °C |
3.47 ft-lb @Temperature 73.4 °F |
Multi-axial, at failure, measured on flat plaques; ASTM D3763 |
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness) AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 4.70 J @Temperature 23.0 °C |
3.47 ft-lb @Temperature 73.4 °F |
Multi-axial, at failure, measured on flat plaques; ASTM D3763 |
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |