Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 35.0 J @Temperature 23.0 °C |
25.8 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron Magnum™ 347EZ ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Impact Test | 35.0 J @Temperature 0.000 °C |
25.8 ft-lb @Temperature 32.0 °F |
Instrumental Falling Weight - Total Penetration Energy; ISO 6603-2 |
Borealis Bormed™ BE860MO Polypropylene Copolymer for Healthcare Applications Bormed BE860MO is a heterophasic copolymer characterized by an excellent impact strength also at low temperatures (deep freeze applications) together with high stiffness and good flow properties.Bor.. |
|||
Impact Test | 35.0 J @Temperature 0.000 °C |
25.8 ft-lb @Temperature 32.0 °F |
Instrumental Falling Weight - Total Penetration Energy; ISO 6603-2 |
Borealis Bormed™ HD850MO Polypropylene Copolymer for Healthcare Applications Bormed HD850MO is a medium melt flow rate polypropylene homo polymer using the Borealis Nucleation Technology (BNT). This provides a polypropylene with excellent dimensional stability and its high c.. |
|||
Impact Test | 35.0 J @Temperature 0.000 °C |
25.8 ft-lb @Temperature 32.0 °F |
Total Penetration Energy; ISO 6603-2 |
Borealis Bormod™ BE961MO Polypropylene for Injection Molding Bormod BE961MO is an heterophasic copolymer characterized by an optimum combination of high stiffness, low creep and very high impact strength.Bormod BE961MO is a new generation grade for very fast .. |