Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Impact Test | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy XTWM206 ASA Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Asia Pacific) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Asia Pacific regio.. |
|||
Impact Test | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Impact Test | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
Multi-axial, at max. load; ASTM D3763 |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |