Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 29.8 J @Temperature -40.0 °C |
22.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 722.MV Molding, extrusion and compounding resin
(discontinued **) Escorene Ultra LD 722.MV is a high vinyl acetate copolymer resin for specialty extrusion and compounding application. Articles made from LD 722.MV are soft and have excellent low temperature toughne.. |
|||
Impact Test | 29.8 J @Temperature -40.0 °C |
22.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 725.21 Molding, extrusion, compounding and adhesive resin
(discontinued **) Escorene Ultra LD 722.21 is 18 wt% vinyl acetate copolymer suitable for molding, extrusion, compounding and hot melt adhesive applications.Information provided by ExxonMobil Chemical |
|||
Impact Test | 29.8 J @Temperature -40.0 °C |
22.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 713.93 Molding, extrusion and compounding resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer with very good toughness, high clarity and excellent processability. It is suitable for use in making molded articles, extruded profile.. |
|||
Impact Test | 29.8 J @Temperature -40.0 °C |
22.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 761.36 Molding, extrusion and compounding resin Escorene Ultra LD 761.36 is a 26.7% vinyl acetate copolymer excellent flexibility and low temperature toughness. LD 761.36 has high filler acceptance.Availability: Latin America, North America and S.. |
|||
Impact Test | 29.8 J @Temperature -40.0 °C |
22.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 783.ND Molding, extrusion and compounding resin
(discontinued **) Escorene Ultra LD 783.ND is a 33% vinyl acetate copolymer suitable for making a variety of specialty molding and extrusion compounds. It has high clarity and a very low modulus.Information provided .. |