Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 22.0 J @Temperature 0.000 °C |
16.2 ft-lb @Temperature 32.0 °F |
Multi-Axial, Ductile; ASTM D3763 |
Flint Hills P9M6K-041A Specialty Impact Copolymer Polypropylene Features: Good clarity and impact resistance. Product does not contain animal derived components.Applications: Injection molding - durable goodsInformation provided by Flint Hills Resources. |
|||
Impact Test | 22.0 J @Temperature 23.0 °C |
16.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Impact Test | 22.0 J @Temperature -40.0 °C |
16.2 ft-lb @Temperature -40.0 °F |
ASTM D3763 |
Diamond Polymers Centrex® 813 General Purpose Injection Molding Grade ASA/AES Centrex 813 resin is a high-gloss, high-impact grade of ASA/AES, a blend of acrylonitrile-styrene-acrylate and acrylonitrile-ethylene-propylene styrene. This injection molding grade with a good bala.. |
|||
Impact Test | 22.0 J @Temperature -30.0 °C |
16.2 ft-lb @Temperature -22.0 °F |
Instrumented Dart Total Energy |
Dow AIM® 4810 High Impact Styrenic Resin AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |