Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented, 2.2 m/s, ductile; ASTM D3763 |
Phillips Sumika Marlex® CBF-300 Talc-Filled High Flow Thermoplastic Olefin
(discontinued **) Applications: Automotive exterior fasciasInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued .. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Prevex VFAX PPE+PS High impact strength. 180F (82C) HDT. Improved productivity/reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 17.0 J @Temperature -30.0 °C |
12.5 ft-lb @Temperature -22.0 °F |
Instrumented Dart Total Energy |
Styron Pulse® 1550 ABS + Polycarbonate, 10% Glass Reinforced PULSE® 1550 Engineering resin is a 10% glass reinforced resin which offers a superior total performance with a balance of high heat resistance, practical toughness and ease of processing.Data pro.. |
|||
Impact Test | 17.0 J @Temperature 23.0 °C |
12.5 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron Pulse® 1550 ABS + Polycarbonate, 10% Glass Reinforced PULSE® 1550 Engineering resin is a 10% glass reinforced resin which offers a superior total performance with a balance of high heat resistance, practical toughness and ease of processing.Data pro.. |
|||
Impact Test | 17.0 J @Thickness 4.00 mm |
12.5 ft-lb @Thickness 0.157 in |
Multi-axial, at max. force; ISO 6603-2 |
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Impact Test | 17.0 J @Thickness 102 mm |
12.5 ft-lb @Thickness 4.00 in |
Multi-axial, at max. load; ASTM D3763 |
Azdel Plus C507-B01 50% Chopped Fiber Mat / PP Resin Matrix (Mineral filled) AZDEL® C507-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu.. |
|||
Impact Test | 17.0 J @Thickness 4.00 mm |
12.5 ft-lb @Thickness 0.157 in |
Multi-axial, at max. load; ASTM D3763 |
Azdel Plus R451-B02 45% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R451-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr.. |
|||
Impact Test | 17.0 J @Thickness 1.70 mm |
12.5 ft-lb @Thickness 0.0669 in |
ASTM D2794-93 |
3M Scotchkote™ 2400 Pipe Renewal Liner 3M Scotchkote Pipe Renewal Liner 2400 has been specifically developed for the rehabilitation of potable water pipe infrastructure to help extend service life, reduce leaks, and improve water quality.. |
|||
Impact Test | 17.0 J @Thickness 4.00 mm |
12.5 ft-lb @Thickness 0.157 in |
Multi-axial, at max. force; ISO 6603-2 |
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |