Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 15.0 J @Temperature -18.0 °C |
11.1 ft-lb @Temperature -0.400 °F |
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763 |
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Impact Test | 15.0 J @Temperature -20.0 °C |
11.1 ft-lb @Temperature -4.00 °F |
Total Penetration Energy; ISO 6603-2 |
Borealis Bormod™ BF970MO Polypropylene for Injection Molding Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o.. |
|||
Impact Test | 15.0 J @Temperature -30.0 °C |
11.1 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
Diamond Polymers Centrex® 835 Sheet Extrusion Grade Centrex 835 resin is a low-gloss grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming applications. Centrex .. |
|||
Impact Test | 15.0 J @Thickness 4.00 mm |
11.1 ft-lb @Thickness 0.157 in |
Multi-axial, at max. force; ISO 6603-2 |
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Impact Test | 15.0 J @Thickness 4.00 mm |
11.1 ft-lb @Thickness 0.157 in |
Multi-axial, at max. force; ISO 6603-2 |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Impact Test | 15.0 J @Thickness 4.00 mm |
11.1 ft-lb @Thickness 0.157 in |
Multi-axial, at max. load; ASTM D3763 |
Azdel Plus R401-B01 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr.. |