Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 47.5 J | 35.0 ft-lb | Oil Quenched at 1218°C; 482°C Temper Temperature |
Latrobe TNWâ„¢ ASTM M10 High Speed Steel TNW is an M10 type high speed steel with a composition that combines the high toughness of a high-molybdenum steel and the excellent wear resistance provided by the 2%
vanadium content. TNW is popul.. |