Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 35.3 J | 26.0 ft-lb | Air Cooled from 1038°C; 593°C Temper Temperature |
Latrobe LSSâ„¢ D7 Tool Steel (ASTM D7) TLS D7 tool steel is a high-carbon, high-chromium air-hardening tool steel that exhibits exceptional wear resistance. The high carbon and vanadium contents result in numerous, hard vanadium carbide .. |
|||
Izod Impact Unnotched | 35.3 J | 26.0 ft-lb | Oil Quenched at 1204°C; 538°C Temper Temperature |
Latrobe Starkâ„¢ ASTM M4 High Speed Steel STARK (M4) is a super high speed steel with very high carbon and vanadium contents for exceptional abrasion resistance. It is well suited for premium cutting tools of all types,
particularly those u.. |
|||
Izod Impact Unnotched | 35.3 J | 26.0 ft-lb | Oil Quenched at 1204°C; 482°C Temper Temperature |
Latrobe Corsairâ„¢ ASTM M3-1 High Speed Steel CORSAIR (M3-1) contains carbon and vanadium levels that are intermediate between those of Double Six (M2) and Crusader (M3-2). This gives the steel a fine balance of wear
resistance and grindability.. |