Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 24.4 J | 18.0 ft-lb | Air Cooled from 788°C; 94°C Temper Temperature |
Latrobe Graph-Air® Cold Work Tool Steel (ASTM A10) Graph-Air tool steel is an air-hardening, graphitic tool steel with outstanding resistance to metal-to-metal sliding wear and galling. The steel contains a uniform dispersion of graphite particles w.. |
|||
Izod Impact Unnotched | 24.4 J | 18.0 ft-lb | Air Cooled from 1010°C; As Quenched |
Latrobe LSSâ„¢ D7 Tool Steel (ASTM D7) TLS D7 tool steel is a high-carbon, high-chromium air-hardening tool steel that exhibits exceptional wear resistance. The high carbon and vanadium contents result in numerous, hard vanadium carbide .. |
|||
Izod Impact Unnotched | 24.4 J | 18.0 ft-lb | Oil Quenched at 1191°C; 622°C Temper Temperature |
Latrobe Dynamax™ ASTM M42, DIN 1.3247 Super High Speed Steel Dynamax super high speed steel is a premium cobalt high speed steel with a chemical composition designed for high hardness and superior hot hardness. These properties make the steel an excellent cho.. |