Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 21.7 J | 16.0 ft-lb | Air Cooled from 1038°C; As Quenched |
Latrobe LSSâ„¢ D7 Tool Steel (ASTM D7) TLS D7 tool steel is a high-carbon, high-chromium air-hardening tool steel that exhibits exceptional wear resistance. The high carbon and vanadium contents result in numerous, hard vanadium carbide .. |