Izod Impact Unnotched 27.1 - 46.1 J
20.0 - 34.0 ft-lb
Carpenter Micro-Melt® T-15 Alloy (AISI T15)
Micro-Melt® T-15 alloy is a high-carbon tungsten-cobalt-vanadium high speed powder metal tool steel possessing excellent abrasion resistance and red hardness. The advantages of Micro-Melt premium p..